全國熱線服務:
新聞資訊 Top label
- The Complete Guide to Pneumatic Cylinders: Selection, Applications, and Technical Considerations
- Understanding N Male Plug Connectors: Applications, Specifications, and Selection Guide
- The Evolution of Smart Sensors: Transforming Industrial Monitoring and Process Control
- Revolutionizing Metal Fabrication: The Essential Guide to Seam Welding Machines
- The Future of Industrial Manufacturing: Cutting Robots Revolutionizing Production Lines
- The Complete Guide to Circulating Ball Mills: Revolutionizing Mineral Processing
Causes of low-temperature embrittlement of high-precision cold-drawn tubes
1. When the dislocations generated by the dislocation source during deformation are blocked by obstacles (such as grain boundaries, second phases, etc.), the local stress exceeds the theoretical strength of the cold-rolled precision bright steel pipe and microcracks occur.
2. Several accumulated dislocations synthesize a microcrack at the grain boundary.
3. Reaction at the intersection of slip zones causes immobile dislocations.